Tc max
50.0 K
Tc ambient
50.0 K
arXiv year
2008
Papers
3
Tc exp.
50.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, arXiv:0806.2195, confirmed by 3 papers
Evidence (6 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 50.0 | — | polycrystal | susceptibility | — | 2010 | T1 | 1003.0273 |
| 50.0 | — | polycrystal | resistivity | — | 2008 | T1 | 0806.2195 |
| 50.0 | — | polycrystal | resistivity | — | 2008 | T1 | DOI: 10.1103/PhysRevLett.101.257002 |
| 48.0 | — | polycrystal | resistivity | — | 2010 | T1 | 1003.0273 |
| 46.0 | — | polycrystal | resistivity | — | 2008 | T1 | DOI: 10.1103/PhysRevLett.101.257002 |
| — | — | polycrystal | specific_heat | — | 2010 | T1 | 1003.0273 |
Structure
- Crystal structure
- ZrCuSiAs structure
- Space group
- P4/nmm
Superconducting parameters
- Hc2
- 345.0 T
- λ_eph (e–ph coupling)
- —
Competing orders
- T_AFM
- 4.0 K
Samples & pressure
- Sample form
- polycrystal
- Doping type
- electron
- Doping level
- 0.200