Tc max
51.0 K
Tc ambient
51.0 K
arXiv year
2008
Papers
10
Tc exp.
51.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.91.024513, confirmed by 2 papers
Evidence (13 records from 10 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 58.0 | — | — | ARPES | — | 2008 | T1 | 0806.2147 |
| 51.0 | — | polycrystal | susceptibility | — | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024513 |
| 50.0 | — | single_crystal | — | — | 2015 | T1 | 1504.04045 |
| 50.0 | — | single_crystal | susceptibility | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.134509 |
| 48.0 | 0.4 | polycrystal | susceptibility | — | 2013 | T1 | DOI: 10.1103/PhysRevB.87.235111 |
| 48.0 | ambient | polycrystal | susceptibility | — | 2013 | T1 | 1303.0917 |
| 47.0 | ambient | single_crystal | specific_heat | — | 2008 | T1 | 0807.4196 |
| 43.0 | — | polycrystal | susceptibility | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.094515 |
| 39.0 | — | single_crystal | susceptibility | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.214509 |
| 34.0 | — | single_crystal | susceptibility | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.020508 |
| 33.5 | — | single_crystal | specific_heat | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.020508 |
| 26.0 | 7.7 | polycrystal | susceptibility | — | 2013 | T1 | DOI: 10.1103/PhysRevB.87.235111 |
| 20.0 | — | polycrystal | susceptibility | — | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024513 |
Structure
- Crystal structure
- tetragonal
- Space group
- P4/nmm
- Lattice c (Å)
- 8.557
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping type
- electron
- Doping level
- 0.100