Tc max
2.2 K
Tc ambient
2.1 K
arXiv year
2007
Papers
6
Tc exp.
2.2 K
Tc theo.
2.1 K
Evidence
experimental
Tc max measured at single_crystal, resistivity, DOI: 10.1103/PhysRevB.82.144532, confirmed by 4 papers
Evidence (10 records from 6 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 2.2 | — | single_crystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.144532 |
| 2.1 | — | single_crystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.144532 |
| 2.1 | — | polycrystal | resistivity | s-wave | 2010 | — | cond-mat/0612605 |
| 2.1 | — | polycrystal | resistivity | — | 2007 | T1 | DOI: 10.1103/PhysRevB.76.214510 |
| 2.1 | — | — | — | — | 2016 | T1 | DOI: 10.1103/PhysRevB.94.144506 |
| 2.1 | — | single_crystal | — | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.144532 |
| 2.1 | — | single_crystal | resistivity, susceptibility, specific_heat | unknown | 2010 | T1 | 1006.5651 |
| 2.1 | — | polycrystal | susceptibility, specific_heat | s-wave | 2010 | — | cond-mat/0612605 |
| 2.1 | — | polycrystal | — | — | 2007 | T1 | DOI: 10.1103/PhysRevB.76.214510 |
| — | — | — | — | s-wave | 2016 | T1 | 1610.00929 |
Structure
- Crystal structure
- orthorhombic
- Space group
- Pmmn (No. 59)
- Lattice a (Å)
- 2.893
- Lattice c (Å)
- 4.705
Superconducting parameters
- Pairing symmetry
- s-wave
- Hc2
- 0.0 T (0 K)
- λ_eph (e–ph coupling)
- 0.52