Tc max
2.9 K
Tc ambient
2.2 K
arXiv year
2009
Papers
2
Tc exp.
2.9 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.79.064508, confirmed by 2 papers
Evidence (2 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 2.9 | — | polycrystal | resistivity | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.064508 |
| 2.2 | — | — | resistivity, susceptibility, muSR | s-wave | 2026 | T1 | 2604.19283 |
Structure
- Crystal structure
- L21
- Space group
- Fm-3m (#225)
- Lattice a (Å)
- 6.536
Superconducting parameters
- λ_eph (e–ph coupling)
- —