Tc max
5.4 K
Tc ambient
5.4 K
arXiv year
2015
Papers
16
Tc exp.
5.4 K
Tc theo.
4.5 K
Evidence
experimental
Tc max measured at single_crystal, susceptibility, DOI: 10.1103/PhysRevB.93.220504, confirmed by 3 papers
Evidence (24 records from 16 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 5.4 | — | single_crystal | susceptibility | s-wave | 2016 | T1 | DOI: 10.1103/PhysRevB.93.220504 |
| 5.4 | — | single_crystal | susceptibility, muSR | s-wave | 2016 | T1 | 1606.01050 |
| 5.4 | ambient | single_crystal | resistivity | — | 2015 | T1 | 1506.05824 |
| 5.3 | — | — | resistivity | — | 2018 | T1 | 1809.08708 |
| 5.2 | ambient | single_crystal | resistivity | s-wave | 2016 | T1 | DOI: 10.1103/PhysRevB.94.024519 |
| 5.0 | ambient | single_crystal | susceptibility | s-wave | 2016 | T1 | DOI: 10.1103/PhysRevB.94.024519 |
| 4.8 | — | single_crystal | muSR | s-wave | 2016 | T1 | DOI: 10.1103/PhysRevB.93.220504 |
| 4.5 | — | single_crystal | susceptibility, resistivity | p-wave | 2026 | T1 | DOI: 10.1103/kcd9-9175 |
| 4.5 | — | single_crystal | resistivity | s-wave | 2020 | T1 | DOI: 10.1103/PhysRevB.101.054514 |
| 4.5 | — | — | — | — | 2019 | T1 | DOI: 10.1103/PhysRevB.99.045110 |
| 4.5 | — | single_crystal | specific_heat | s-wave | 2020 | T1 | DOI: 10.1103/PhysRevB.101.054514 |
| 4.5 | — | single_crystal | susceptibility | s-wave | 2020 | T1 | DOI: 10.1103/PhysRevB.101.054514 |
| 4.0 | — | thin_film | resistivity | — | 2020 | T1 | DOI: 10.1103/PhysRevB.102.014420 |
| 4.0 | 1.7 | single_crystal | resistivity | — | 2019 | T1 | DOI: 10.1103/PhysRevB.99.054501 |
| 2.5 | 42.9 | single_crystal | resistivity | — | 2019 | T1 | DOI: 10.1103/PhysRevB.99.054501 |
| 2.4 | 1.3 | single_crystal | resistivity | — | 2019 | T1 | DOI: 10.1103/PhysRevB.99.054501 |
| 1.7 | — | single_crystal | resistivity | s-wave | 2017 | T1 | DOI: 10.1103/PhysRevB.95.134519 |
| 1.7 | — | single_crystal | susceptibility | s-wave | 2017 | T1 | DOI: 10.1103/PhysRevB.95.134519 |
| 1.6 | ambient | single_crystal | resistivity, susceptibility | — | 2019 | T1 | DOI: 10.1103/PhysRevB.99.054501 |
| 1.3 | — | single_crystal | muSR | s-wave | 2021 | T1 | DOI: 10.1103/PhysRevLett.127.217002 |
| — | — | thin_film | — | — | 2024 | — | 2411.05551 |
| — | — | thin_film | STM | nodal | 2024 | — | 2411.09239 |
| — | — | — | STM | s-wave | 2017 | T1 | 1708.08204 |
| — | ambient | — | ARPES | — | 2015 | T1 | 1505.07231 |
Structure
- Crystal structure
- tetragonal
- Space group
- I4/mmm
- Lattice a (Å)
- 3.360
- Lattice c (Å)
- 12.980
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- λ_eph (e–ph coupling)
- 0.54
Samples & pressure
- Sample form
- single_crystal
- Substrate
- MgO
- Pressure type
- none
- Doping type
- none