Tc max
12.4 K
Tc ambient
—
arXiv year
2019
Papers
1
Tc max measured at polycrystal, resistivity, arXiv:1901.08633
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 12.4 | — | polycrystal | resistivity, susceptibility, specific_heat | — | 2019 | — | 1901.08633 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —