Tc max
6.8 K
Tc ambient
6.8 K
arXiv year
2014
Papers
5
Tc exp.
6.8 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.97.020502, confirmed by 2 papers
Evidence (7 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 6.8 | — | polycrystal | resistivity | s-wave | 2018 | T1 | DOI: 10.1103/PhysRevB.97.020502 |
| 6.8 | — | polycrystal | resistivity | s-wave | 2018 | T1 | 1801.01955 |
| 6.0 | — | polycrystal | resistivity, susceptibility, specific_heat, muSR | s-wave | 2018 | T1 | DOI: 10.1103/PhysRevB.97.020502 |
| 6.0 | — | polycrystal | resistivity, susceptibility, specific_heat, muSR | s-wave | 2018 | T1 | 1801.01955 |
| — | — | polycrystal | muSR | — | 2018 | T1 | DOI: 10.1103/PhysRevB.97.100505 |
| — | — | — | muSR | — | 2018 | T1 | 1801.02841 |
| — | — | — | — | — | 2014 | T1 | 1407.8416 |
Structure
- Crystal structure
- alpha-Mn
- Space group
- I-43m
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- Hc2
- 11.2 T (0 K)
- λ_eph (e–ph coupling)
- 1.20
Samples & pressure
- Sample form
- polycrystal