Tc max
8.1 K
Tc ambient
8.1 K
arXiv year
2020
Papers
2
Tc exp.
8.1 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, arXiv:2004.03834, confirmed by 2 papers
Evidence (6 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 8.1 | — | polycrystal | resistivity | s-wave | 2020 | — | 2004.03834 |
| 8.1 | — | polycrystal | resistivity | s-wave | 2020 | T1 | DOI: 10.1103/PhysRevB.101.144508 |
| 8.0 | — | polycrystal | resistivity, susceptibility, muSR | s-wave | 2020 | — | 2004.03834 |
| 8.0 | — | polycrystal | resistivity, susceptibility | s-wave | 2020 | T1 | DOI: 10.1103/PhysRevB.101.144508 |
| 7.9 | — | polycrystal | specific_heat | s-wave | 2020 | — | 2004.03834 |
| 7.9 | — | polycrystal | specific_heat | s-wave | 2020 | T1 | DOI: 10.1103/PhysRevB.101.144508 |
Structure
- Crystal structure
- cubic α-Mn
- Space group
- I4̅3m
- Lattice a (Å)
- 9.628
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- Hc2
- 22.1 T (0 K)
- λ_eph (e–ph coupling)
- 0.73
Competing orders
- ρ(T) exponent
- 2.00
Samples & pressure
- Sample form
- polycrystal