Tc max
8.1 K
Tc ambient
8.1 K
arXiv year
2024
Papers
2
Tc exp.
8.1 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, arXiv:2401.07614, confirmed by 2 papers
Evidence (5 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 8.1 | — | polycrystal | resistivity | — | 2024 | T1 | 2401.07614 |
| 8.1 | — | polycrystal | resistivity | s-wave | 2024 | T1 | DOI: 10.1103/PhysRevB.109.174518 |
| 7.7 | — | polycrystal | susceptibility, specific_heat, muSR | s-wave | 2024 | T1 | 2401.07614 |
| 7.7 | — | polycrystal | susceptibility | s-wave | 2024 | T1 | DOI: 10.1103/PhysRevB.109.174518 |
| 7.5 | — | polycrystal | specific_heat | s-wave | 2024 | T1 | DOI: 10.1103/PhysRevB.109.174518 |
Structure
- Crystal structure
- α-Mn cubic
- Space group
- I43m
- Lattice a (Å)
- 9.654
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- Hc2
- 17.9 T (0 K, from resistivity)
- λ_eph (e–ph coupling)
- 0.73
Samples & pressure
- Sample form
- polycrystal