Tc max
40.0 K
Tc ambient
40.0 K
Discovery
2002
Papers
1
Tc max measured at ambient, polycrystal, susceptibility, arXiv:cond-mat/0205487
Evidence (4 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 40.0 | ambient | polycrystal | susceptibility | — | 2002 | cond-mat/0205487 |
| 37.0 | ambient | polycrystal | susceptibility | — | 2002 | cond-mat/0205487 |
| 26.0 | ambient | polycrystal | susceptibility | — | 2002 | cond-mat/0205487 |
| 17.0 | ambient | polycrystal | susceptibility | — | 2002 | cond-mat/0205487 |
Structure
- Crystal structure
- I4/mmm
- Space group
- I4/mmm
- Lattice a (Å)
- 3.839
- Lattice c (Å)
- 28.591
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping level
- 0.112