Tc max
8.0 K
Tc ambient
—
arXiv year
2000
Papers
5
Tc exp.
8.0 K
Tc theo.
11.7 K
Evidence
theoretical
Tc max measured at P=150 GPa, susceptibility, arXiv:cond-mat/0108267, confirmed by 3 papers
Evidence (20 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 11.7 | 103.1 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 11.3 | 128.6 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 10.5 | 103.1 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 10.1 | 118.2 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 10.0 | 120.0 | — | — | — | 2001 | T1 | DOI: 10.1103/PhysRevB.63.104516 |
| 9.9 | 128.6 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 9.5 | 149.6 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 8.8 | 118.2 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 8.1 | 149.6 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 8.0 | 165.6 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 8.0 | 150.0 | — | susceptibility | — | 2001 | T2 | cond-mat/0108267 |
| 7.5 | 160.0 | — | susceptibility | — | 2002 | T3 | cond-mat/0201520 |
| 6.6 | 165.6 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 6.0 | 25.0 | — | susceptibility | — | 2001 | T2 | cond-mat/0108267 |
| 5.8 | 25.0 | polycrystal | resistivity | — | 2002 | T1 | DOI: 10.1103/PhysRevB.65.064504 |
| 5.1 | 103.1 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 5.0 | 118.2 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 4.0 | 103.1 | — | — | — | 2000 | T2 | cond-mat/0011274 |
| 4.0 | 15.0 | — | susceptibility | — | 2001 | T2 | cond-mat/0108267 |
| 3.9 | 118.2 | — | — | — | 2000 | T2 | cond-mat/0011274 |
Structure
- Crystal structure
- bcc
- Space group
- Im-3m
- Phase
- 1313
Superconducting parameters
- λ_eph (e–ph coupling)
- 0.92
- ω_log
- 265 K