Tc max
23.0 K
Tc ambient
20.0 K
arXiv year
1990
Papers
2
Tc exp.
23.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevLett.65.3201, confirmed by 2 papers
Evidence (2 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 23.0 | — | polycrystal | resistivity | — | 1990 | T1 | DOI: 10.1103/PhysRevLett.65.3201 |
| 20.0 | — | polycrystal | resistivity | — | 1991 | T1 | DOI: 10.1103/PhysRevB.43.12935 |
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.150