Tc max
55.2 K
Tc ambient
55.2 K
arXiv year
2008
Papers
9
Tc exp.
55.2 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, polycrystal, resistivity, arXiv:0806.0980, confirmed by 2 papers
Evidence (13 records from 9 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 55.2 | ambient | polycrystal | resistivity | — | 2008 | T1 | 0806.0980 |
| 55.2 | — | polycrystal | resistivity | unknown | 2008 | T1 | DOI: 10.1103/PhysRevB.78.092504 |
| 55.0 | — | polycrystal | magnetization | — | 2008 | T1 | 0806.0980 |
| 55.0 | — | polycrystal | susceptibility | unknown | 2008 | T1 | DOI: 10.1103/PhysRevB.78.092504 |
| 52.2 | — | polycrystal | resistivity | — | 2009 | T1 | 0904.3625 |
| 52.2 | ambient | polycrystal | resistivity | — | 2008 | T1 | 0806.0980 |
| 52.2 | — | polycrystal | resistivity | unknown | 2008 | T1 | DOI: 10.1103/PhysRevB.78.092504 |
| 52.0 | — | — | STM | s_pm | 2010 | T1 | 1007.3151 |
| 51.5 | — | polycrystal | STM, susceptibility | d-wave | 2008 | T1 | 0806.1986 |
| 17.0 | — | single_crystal | resistivity | — | 2011 | T1 | 1102.3312 |
| 17.0 | — | polycrystal | susceptibility | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.014503 |
| — | — | single_crystal | susceptibility | — | 2013 | T1 | 1303.2767 |
| — | ambient | polycrystal | specific_heat, susceptibility | — | 2008 | T1 | 0812.1188 |
Structure
- Crystal structure
- Cmma
- Space group
- Cmma
- Lattice a (Å)
- 5.553
- Lattice c (Å)
- 8.453
Superconducting parameters
- Hc2
- 312.0 T (0 K, WHH formula)
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping type
- electron
- Doping level
- 0.100