Tc max
50.0 K
Tc ambient
50.0 K
arXiv year
2008
Papers
1
Tc max measured at polycrystal, resistivity, arXiv:0804.2105
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 50.0 | — | polycrystal | resistivity | — | 2008 | — | 0804.2105 |
Structure
- Crystal structure
- ZrCuSiAs-type
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- SDW
- ρ(T) exponent
- 1.00
Samples & pressure
- Sample form
- polycrystal
- Doping type
- electron
- Doping level
- 0.500