Tc max
12.6 K
Tc ambient
12.6 K
arXiv year
2000
Papers
3
Tc exp.
12.6 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.64.064502, confirmed by 2 papers
Evidence (7 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 12.6 | — | polycrystal | resistivity | — | 2001 | T1 | DOI: 10.1103/PhysRevB.64.064502 |
| 12.5 | — | polycrystal | resistivity | — | 2001 | T1 | DOI: 10.1103/PhysRevB.64.064502 |
| 12.0 | — | polycrystal | resistivity | — | 2001 | T1 | DOI: 10.1103/PhysRevB.64.064502 |
| 12.0 | — | polycrystal | susceptibility | — | 2000 | T1 | DOI: 10.1103/PhysRevB.62.R11977 |
| 10.5 | — | polycrystal | resistivity | — | 2001 | T1 | DOI: 10.1103/PhysRevB.64.064502 |
| 10.1 | — | polycrystal | resistivity | — | 2001 | T1 | DOI: 10.1103/PhysRevB.64.064502 |
| — | — | — | — | — | 2022 | T1 | 2209.05198 |
Structure
- Crystal structure
- distorted perovskite
- Lattice a (Å)
- 5.940
- Lattice c (Å)
- 8.430
Superconducting parameters
- λ_eph (e–ph coupling)
- 1.22
Samples & pressure
- Sample form
- polycrystal
- Doping type
- hole
- Doping level
- 0.600