Tc max
42.0 K
Tc ambient
26.0 K
arXiv year
2007
Papers
12
Tc exp.
42.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.77.224503, confirmed by 2 papers
Evidence (12 records from 12 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 42.0 | — | polycrystal | susceptibility | — | 2008 | T1 | DOI: 10.1103/PhysRevB.77.224503 |
| 42.0 | — | powder | susceptibility | — | 2007 | T1 | 0710.0773 |
| 26.0 | — | thin_film | resistivity | — | 2009 | T1 | DOI: 10.1103/PhysRevB.80.024501 |
| 25.0 | — | thin_film | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.035149 |
| 25.0 | — | thin_film | resistivity, ARPES | d-wave | 2012 | T1 | DOI: 10.1103/PhysRevLett.109.267001 |
| 22.0 | — | thin_film | resistivity | — | 2012 | T1 | DOI: 10.1103/PhysRevB.85.024519 |
| 19.0 | — | thin_film | resistivity | — | 2011 | T1 | DOI: 10.1103/PhysRevB.84.214507 |
| 19.0 | — | thin_film | resistivity | — | 2011 | T1 | 1111.7079 |
| 18.0 | — | thin_film | resistivity | d-wave | 2012 | T1 | DOI: 10.1103/PhysRevB.86.094509 |
| 18.0 | — | — | resistivity | d-wave | 2012 | T1 | 1203.5237 |
| — | — | thin_film | STM | — | 2020 | T1 | DOI: 10.1103/PhysRevLett.125.077002 |
| — | — | thin_film | resistivity | — | 2016 | T1 | DOI: 10.1103/PhysRevB.94.054504 |
Structure
- Crystal structure
- infinite-layer
- Phase
- infinite_layer
Superconducting parameters
- Pairing symmetry
- d-wave
- Gap structure
- nodal
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- thin_film
- Substrate
- SrTiO3
- Doping type
- electron
- Doping level
- 0.150