Tc max
13.2 K
Tc ambient
13.2 K
arXiv year
2008
Papers
1
Tc exp.
13.2 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, arXiv:0807.2223
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 13.2 | — | polycrystal | susceptibility, specific_heat | — | 2008 | T1 | 0807.2223 |
Structure
- Lattice a (Å)
- 3.929
- Lattice c (Å)
- 12.270
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping level
- 0.300