Tc max
33.0 K
Tc ambient
33.0 K
arXiv year
2011
Papers
10
Tc exp.
33.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, NMR, arXiv:1509.04382, confirmed by 4 papers
Evidence (15 records from 10 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 33.0 | — | single_crystal | NMR | s_pm | 2015 | T1 | 1509.04382 |
| 33.0 | — | single_crystal | susceptibility | — | 2014 | T1 | 1408.1531 |
| 33.0 | — | single_crystal | susceptibility, specific_heat | s_pm | 2013 | T1 | DOI: 10.1103/PhysRevB.87.174520 |
| 33.0 | — | single_crystal | susceptibility, specific_heat | s_pm | 2013 | T1 | 1305.2074 |
| 30.0 | — | single_crystal | susceptibility | — | 2013 | T1 | 1312.4687 |
| 30.0 | — | single_crystal | resistivity, susceptibility | — | 2011 | T1 | 1112.3743 |
| 26.0 | — | single_crystal | NMR | s_pm | 2015 | T1 | 1509.04382 |
| 26.0 | — | single_crystal | susceptibility | s_pm | 2013 | T1 | DOI: 10.1103/PhysRevB.87.174520 |
| 26.0 | — | single_crystal | susceptibility | s_pm | 2013 | T1 | 1305.2074 |
| 26.0 | — | single_crystal | resistivity, specific_heat | unknown | 2012 | T1 | DOI: 10.1103/PhysRevB.85.144515 |
| 26.0 | — | single_crystal | specific_heat, muSR | s_pm | 2011 | T1 | 1108.4480 |
| 25.0 | — | single_crystal | resistivity, susceptibility | — | 2013 | T1 | 1301.6142 |
| 23.0 | — | single_crystal | specific_heat | s_pm | 2013 | T1 | DOI: 10.1103/PhysRevB.87.174520 |
| 23.0 | — | single_crystal | specific_heat | s_pm | 2013 | T1 | 1305.2074 |
| — | — | single_crystal | ARPES | s_pm | 2019 | T1 | 1911.04308 |
Structure
- Crystal structure
- I4/mmm
- Space group
- I4/mmm
- Lattice a (Å)
- 3.920
- Lattice c (Å)
- 12.230
Superconducting parameters
- Pairing symmetry
- s_pm
- Gap structure
- nodal
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- AFM
- ρ(T) exponent
- 1.00
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none
- Doping type
- isovalent
- Doping level
- 0.350