Tc max
30.0 K
Tc ambient
30.0 K
arXiv year
2016
Papers
13
Tc exp.
30.0 K
Tc theo.
10.0 K
Evidence
experimental
Tc max measured at polycrystal, resistivity, arXiv:1706.03641, confirmed by 7 papers
Evidence (16 records from 13 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 30.0 | ambient | polycrystal | — | s_pm | 2018 | T1 | DOI: 10.1103/PhysRevB.97.140506 |
| 30.0 | — | — | resistivity, susceptibility | — | 2018 | T1 | 1805.12276 |
| 30.0 |
Structure
- Crystal structure
- ZrCuSiAs-type
- Space group
- P4/nmm
- Lattice a (Å)
- 4.037
- Lattice c (Å)
- 8.526
Superconducting parameters
- Pairing symmetry
- s_pm
- Gap structure
- multi_gap
- Hc2
- 8.0 T (at 26 K)
- λ_eph (e–ph coupling)
- 0.40
- ω_log
- 213 K
Competing orders
- ρ(T) exponent
- 1.30
Samples & pressure
- Sample form
- polycrystal
- Doping type
- none