Tc max
128.0 K
Tc ambient
128.0 K
arXiv year
2004
Papers
1
Tc exp.
128.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.70.092501
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 128.0 | — | polycrystal | susceptibility | — | 2004 | T1 | DOI: 10.1103/PhysRevB.70.092501 |
Structure
- Crystal structure
- tetragonal
- Space group
- P4/mmm
- Phase
- 1234
- Lattice a (Å)
- 3.849
- Lattice c (Å)
- 19.005
Superconducting parameters
- Pairing symmetry
- d-wave
- Hc2
- 207.0 T (0 K, H parallel c, clean limit)
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal