Tc max
82.0 K
Tc ambient
82.0 K
arXiv year
1990
Papers
2
Tc exp.
82.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.41.11209, confirmed by 2 papers
Evidence (2 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 82.0 | — | polycrystal | resistivity | — | 1990 | T1 | DOI: 10.1103/PhysRevB.41.11209 |
| 80.5 | ambient | powder | susceptibility | — | 2001 | T2 | cond-mat/0107538 |
Structure
- Crystal structure
- orthorhombic
- Lattice a (Å)
- 3.805
- Lattice c (Å)
- 27.122
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping level
- 0.200