Tc max
80.0 K
Tc ambient
80.0 K
arXiv year
1994
Papers
2
Tc exp.
80.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, polycrystal, susceptibility, DOI: 10.1103/PhysRevB.59.11205
Evidence (3 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 80.0 | ambient | polycrystal | susceptibility | — | 1999 | T1 | DOI: 10.1103/PhysRevB.59.11205 |
| 6.0 | ambient | polycrystal | susceptibility | — | 1999 | T1 | DOI: 10.1103/PhysRevB.59.11205 |
| — | ambient | polycrystal | resistivity | — | 1994 | T1 | DOI: 10.1103/PhysRevB.50.10265 |
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.350