Tc max
95.0 K
Tc ambient
90.5 K
arXiv year
1987
Papers
5
Tc exp.
95.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.39.12290, confirmed by 3 papers
Evidence (13 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 95.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 93.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 92.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 90.5 | — | polycrystal | resistivity | — | 1988 | T1 | DOI: 10.1103/PhysRevB.38.8931 |
| 90.0 | — | polycrystal | susceptibility, resistivity | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.6667 |
| 81.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 69.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 50.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 37.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 19.0 | — | polycrystal | susceptibility | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.12290 |
| 4.2 | — | polycrystal | susceptibility, resistivity | — | 1989 | T1 | DOI: 10.1103/PhysRevB.39.6667 |
| — | 0.0 | polycrystal | — | — | 1990 | T1 | DOI: 10.1103/PhysRevB.41.2103 |
| — | — | polycrystal | susceptibility | — | 1987 | T1 | DOI: 10.1103/PhysRevB.36.7230 |
Structure
- Crystal structure
- orthorhombic
- Phase
- cuprate_123
- Lattice a (Å)
- 3.845
- Lattice c (Å)
- 11.678
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping type
- isovalent
- Doping level
- 0.050