Tc max
7.2 K
Tc ambient
7.2 K
arXiv year
2018
Papers
3
Tc exp.
7.2 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.106.014507
Evidence (9 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 7.2 | — | polycrystal | resistivity | — | 2022 | T1 | DOI: 10.1103/PhysRevB.106.014507 |
| 6.8 | — | polycrystal | resistivity | — | 2022 | T1 | DOI: 10.1103/PhysRevB.106.014507 |
| 6.4 |
Structure
- Crystal structure
- Mn5Si3-type
- Space group
- P6_3/mcm (#193)
- Lattice a (Å)
- 8.182
- Lattice c (Å)
- 5.384
Superconducting parameters
- Hc2
- 7.2 T (zero-temperature)
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal