Tc max
1.0 K
Tc ambient
1.0 K
Discovery
2001
Papers
21
Tc max measured at ambient, arXiv:cond-mat/0107304, confirmed by 3 papers
Evidence (22 records from 21 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 10.0 | ambient | — | — | s-wave | 2001 | cond-mat/0107610 |
| 1.0 | ambient | — | — | p-wave | 2002 | cond-mat/0204440 |
| 1.0 | ambient | — | — | p-wave | 2001 | cond-mat/0107304 |
| 0.6 | ambient | single_crystal | resistivity, susceptibility | — | 2005 | cond-mat/0502341 |
| 0.6 | ambient | single_crystal | — | p-wave | 2002 | cond-mat/0207285 |
| 0.3 | ambient | — | — | p-wave | 2003 | cond-mat/0304532 |
| 0.3 | ambient | — | — | s-wave | 2001 | cond-mat/0107610 |
| 0.3 | ambient | — | — | p-wave | 2002 | cond-mat/0212520 |
| — | — | — | — | — | 2005 | cond-mat/0505123 |
| — | — | — | — | p-wave | 2004 | cond-mat/0404261 |
| — | — | — | — | p-wave | 2004 | cond-mat/0405461 |
| — | ambient | — | — | — | 2004 | cond-mat/0406371 |
| — | — | — | — | p-wave | 2004 | cond-mat/0411503 |
| — | — | — | specific_heat | — | 2003 | cond-mat/0302449 |
| — | ambient | — | — | p-wave | 2003 | cond-mat/0312378 |
| — | — | — | — | p-wave | 2002 | cond-mat/0203309 |
| — | — | single_crystal | — | p-wave | 2002 | cond-mat/0206534 |
| — | ambient | — | — | — | 2002 | cond-mat/0209237 |
| — | — | — | — | — | 2002 | cond-mat/0210552 |
| — | — | — | — | — | 2002 | cond-mat/0211519 |
| — | — | — | — | — | 2001 | cond-mat/0105627 |
| — | — | — | — | — | 2001 | cond-mat/0111292 |
Structure
- Crystal structure
- C15 cubic Laves crystal structure
- Space group
- O_h (m3m)
- Lattice a (Å)
- 7.393
Superconducting parameters
- Pairing symmetry
- p-wave
- Gap structure
- nodal
- Hc2
- 0.9 T (T=0.05 K)
- λ_eph (e–ph coupling)
- 1.00
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none