Determination of I-V Curves of HTS Tapes From The Frequency Dependent AC Transport Loss
Eduard Demenčík, Aurelien Godfrin, Víctor Zermeño, Francesco Grilli
arXiv:1511.08347 · DOI 10.1109/TASC.2016.2529853 · 2015-11-26 · arXiv: Superconductivity
Active bibliographic source — not scientific approval
Bibliographic access preserves source history; it does not approve extracted materials or validate reported claims. Review warnings on each occurrence separately.
Abstract
The current-voltage characteristics of superconductors are commonly determined by means of a standard 4-probe DC measurement technique. In coated conductors, however, one often encounters problems due to weak or no stabilization and in such case, when the risk of burning the tape is high, the 4-probe approach can fail. In other cases such as in HTS cable structures, besides vulnerability and high risk of damage, it may also be difficult to achieve a high critical current level with a power supply that is normally used to characterize single strands. We therefore investigated an alternative method to determine the DC I-V curve, based on measuring the AC transport loss as a function of frequency in overcritical current range. In the AC regime, both the hysteretic loss component and the joule dissipation are present for applied transport currents exceeding the critical current Ic. In this work, AC loss measurements at different frequencies are related to different electric fields in DC and a curve similar to the DC I-V is obtained. From this curve, the power index N and Ic values are estimated. AC regime operation can be more beneficial for two reasons: firstly, because very high currents can be achieved easily by using a transformer; secondly, because the effective joule heat dissipation with overcritical AC currents is much lower than that with DC of the same amplitudes. In the experiment, we used a 4 mm wide YBCO reference tape with 20 μm of Cu-stabilization. For the comparison with AC transport loss, the sample was measured with the standard 4-probe technique and remained stable even in overload condition. To support our study, numerical simulations, reproducing both transient and stationary operation conditions, were performed. A similar relation between the AC current transport loss and the I-V curves was also observed in the simulations.
Similar papers
Influence of the voltage taps position on the self-field DC and AC transport characterization of HTS superconducting tapes
similarity 0.90M. Vojenciak et al. · 2013 · arXiv:1308.3045
Source status unknown — claims are unverified
Effect of combining a DC bias current with an AC transport current on AC losses in a High Temperature Superconductor
similarity 0.90Patricia Dolez et al. · 1998 · arXiv:cond-mat/9811269
Source status unknown — claims are unverified
Superconducting Cables Characterization with an electrical method
similarity 0.89L. Morici et al. · 2018 · arXiv:1809.07145
Source status unknown — claims are unverified
Numerical evaluation of AC losses in an HTS insert coil for high field magnet during its energization
similarity 0.89K. Kajikawa et al. · 2014 · arXiv:1405.7765
Source status unknown — claims are unverified
Review of the AC Loss Computation for HTS using the H-formulation
similarity 0.87Boyang Shen et al. · 2019 · arXiv:1908.02176
Source status unknown — claims are unverified
DC Characterization of a Circular, Epoxy-Impregnated High Temperature Superconducting (HTS) Coil
similarity 0.87Di Hu et al. · 2015 · arXiv:1512.07900
Source status unknown — claims are unverified