Chemical stability and superconductivity in Ag-sheathed CaKFe4As4 superconducting tapes
Zhe Cheng, Chiheng Dong, He Huang, Shifa Liu, Yanchang Zhu, Dongliang Wang, Vitalii Vlasko-Vlasov, Ulrich Welp, Wai-Kwong Kwok, Yanwei Ma
arXiv:1809.03768 · DOI 10.1088/1361-6668/aaedff · 2018-09-11 · Superconductor Science and Technology
Active bibliographic source — not scientific approval
Bibliographic access preserves source history; it does not approve extracted materials or validate reported claims. Review warnings on each occurrence separately.
Abstract
Ag-sheathed CaKFe4As4 superconducting tapes have been fabricated via the ex-situ powder-in-tube method. Thermal and X-ray diffraction analyses suggest that the CaKFe4As4 phase is unstable at high temperatures. It decomposes into the CaAgAs phase which reacts strongly with the silver sheath. We therefore sintered the tape at 500C and obtain a transport critical current density Jc(4.2 K, 0 T)~ 2.7x10^4 A/cm2. The pinning potential derived from magnetoresistance measurements is one order of magnitude lower than that of the (Ba/Sr)1-xKxFe2As2 tapes. Combining with the scanning electron microscopy and magneto-optical imaging results, we suggest that bad connectivity between superconducting grains caused by the low sintering temperature is the main factor responsible for the low Jc. However, this system is still a promising candidate for superconducting wires and tapes if we further optimize the post-annealing process to achieve better grain connectivity.
Source-reported materials — not catalogue approval
| Formula | Reported Tc (K) | Pressure (GPa) | Type |
|---|---|---|---|
| CaKFe4As4 Archive — visibility unverified Source-occurrence policy only; no material identity or catalogue acceptance is inferred from the formula. | — | Pressure not reported | — |
Similar papers
Large transport critical currents of powder-in-tube Sr0.6K0.4Fe2As2/Ag superconducting wires and tapes
similarity 0.90Lei Wang et al. · 2009 · arXiv:0911.3701
Source status unknown — claims are unverified
Superconducting properties and magneto-optical imaging of Ba0.6K0.4Fe2As2 PIT wires with Ag addition
similarity 0.88Qing-Ping Ding et al. · 2012 · arXiv:1201.5201
Source status unknown — claims are unverified
High-performance Ba1-xKxFe2As2 superconducting tapes with grain texture engineered via a scalable and cost-effective fabrication
similarity 0.88Shifa Liu et al. · 2021 · arXiv:2102.10829
Source status unknown — claims are unverified
High critical current density and low anisotropy in textured Sr1-xKxFe2As2 tapes for high field applications
similarity 0.88Zhaoshun Gao et al. · 2013 · arXiv:1302.4583
Source status unknown — claims are unverified
Large Transport Critical Current Densities of Ag Sheathed (Ba,K)Fe2As2+Ag Superconducting Wires Fabricated by an ex-situ Powder-in-Tube (PIT) Process
similarity 0.88Kazumasa Togano et al. · 2011 · arXiv:1103.1701
Source status unknown — claims are unverified
Achievement of practical level critical current densities in PIT Ba1-xKxFe2As2/Ag tapes by conventional cold mechanical deformation
similarity 0.87Zhaoshun Gao et al. · 2013 · arXiv:1310.4623
Source status unknown — claims are unverified