← Back to search

Effect of Etching Methods on Dielectric Losses in Transmons

T. A. Chudakova, G. S. Mazhorin, I. V. Trofimov, N. Yu. Rudenko, A. M. Mumlyakov, A. S. Kazmina, E. Yu. Egorova, P. A. Gladilovich, M. V. Chichkov, N. A. Maleeva, M. A. Tarkhov, V. I. Chichkov

arXiv:2409.16097 · DOI 10.1134/S0021364024602410 · 2024-09-24 · JETP Letters

T3experimental1 citations

Active bibliographic source — not scientific approval

Bibliographic access preserves source history; it does not approve extracted materials or validate reported claims. Review warnings on each occurrence separately.

Abstract

Superconducting qubits are considered as a promising platform for implementing a fault tolerant quantum computing. However, surface defects of superconductors and the substrate leading to qubit state decoherence and fluctuations in qubit parameters constitute a significant problem. The amount and type of defects depend both on the chip materials and fabrication procedure. In this work, transmons produced by two different methods of aluminum etching: wet etching in a solution of weak acids and dry etching using a chlorine-based plasma are experimentally studied. The relaxation and coherence times for dry-etched qubits are more than twice as long as those for wet-etched ones. Additionally, the analysis of time fluctuations of qubit frequencies and relaxation times, which is an effective method to identify the dominant dielectric loss mechanisms, indicates a significantly lower impact of two-level systems in the dry-etched qubits compared to the wet-etched ones.