Role of grain size in superconducting boron-doped nanocrystalline diamond thin films grown by CVD

Gufei Zhang, S. D. Janssens, J. Vanacken, M. Timmermans, J. Vacík, G. W. Ataklti, W. Decelle, W. Gillijns, B. Goderis, K. Haenen, P. Wagner, V. V. Moshchalkov

DOI 10.1103/PhysRevB.84.214517 · Physical Review B

T1

Active bibliographic source — not scientific approval

Bibliographic access preserves source history; it does not approve extracted materials or validate reported claims. Review warnings on each occurrence separately.

Abstract

The grain size dependence of the superconducting transition, the normal state resistivity, and the insulating behavior at high magnetic fields are studied on a series of boron-doped nanocrystalline diamond (B:NCD) thin films with different grain sizes. The systematic change of the grain size is achieved by varying the methane-to-hydrogen ratio (C/H ratio) for the growth of different B:NCD films. Even though a fixed trimethylboron- (TMB) to-methane gas ratio is supposed to induce the identical boron-doping level in all the B:NCD films, the boron concentration and the carrier density are found to be a decreasing function of the grain size. Another consequence of the increase in grain size is the decreasing grain boundary density. These two concurrent consequences of the chemical vapor deposition mode of B:NCD are responsible for the grain size dependence of the critical temperature TC, the localization radius aH at the boron site, the normal state resistivity ρnorm, the Hall mobility μH, the Ioffe-Regel product kFl, the HC2-T phase boundary, and the coherence length ξGL.

Source-reported materials — not catalogue approval

FormulaReported Tc (K)Pressure (GPa)Type
B:NCD

Archive — visibility unverified

Source-occurrence policy only; no material identity or catalogue acceptance is inferred from the formula.

—Pressure not reportedunknown

Similar papers