Abstract
Bi2Sr2CaCu2O8+x (Bi-2212) superconducting long-length wires are mainly limited in obtaining high critical currents densities (JC) by the internal gas pressure generated during the heat treatment, which expands the wire diameter and dedensifies the superconducting filaments. Several ways have been developed to increase the density of the superconducting filaments and therefore decreasing the bubble density: much higher critical currents have been reached always acting on the final as-drawn wires. We here try to pursue the same goal of having a denser wire by acting on the deformation technique, through a partial use of the groove-rolling at different wire processing stages. Such technique has a larger powders compaction power, is straightforwardly adaptable to long length samples, and allows the fabrication of samples with round, square or rectangular shape depending on the application requirements. In this paper we demonstrate the capability of this technique to increase the density in Bi-2212 wires which leads to a three-fold increase in Jc with respect to drawn wires, making this approach very promising for fabricating Bi-2212 wires for high magnetic field magnets, i.e. above 25 T.
Source-reported materials — not catalogue approval
| Formula | Reported Tc (K) | Pressure (GPa) | Type |
|---|---|---|---|
| Bi2Sr2CaCu2O8+x Archive — visibility unverified Source-occurrence policy only; no material identity or catalogue acceptance is inferred from the formula. | — | Pressure not reported | unknown |
Similar papers
New concept for the development of Bi-2212 wires for high field applications
similarity 0.94Andrea Malagoli et al. · 2015 · arXiv:1510.03344
Source status unknown — claims are unverified
Comparison of grain texture in round Bi2212 and flat Bi2223 superconducting wires and its relation to high critical current densities
similarity 0.87F. Kametani et al. · 2014 · arXiv:1409.8216
Source status unknown — claims are unverified
Reduction of gas bubbles and improved critical current density in Bi-2212 round wire by swaging
similarity 0.87Jianyi Jiang et al. · 2013 · arXiv:1301.3401
Source status unknown — claims are unverified
Investigation of inter-grain critical current density in Bi2Sr2CaCu2O8+d superconducting wires and its relationship with the heat treatment protocol
similarity 0.87I. Pallecchi et al. · 2017 · arXiv:1707.02891
Source status unknown — claims are unverified
Superconducting properties of strongly underdoped Bi2Sr2CaCu2O8+x single crystals
similarity 0.85M. Li et al.
Source status unknown — claims are unverified
Crystal Growth and High-Pressure Effects of Bi-Based Superconducting Whiskers
similarity 0.83Ryo Matsumoto et al. · 2021 · arXiv:2104.01602
Source status unknown — claims are unverified