Tc max
96.0 K
Tc ambient
95.0 K
arXiv year
1988
Papers
1059
Tc exp.
96.0 K
Tc theo.
120.0 K
Evidence
experimental
Tc max measured at single_crystal, resistivity, DOI: 10.1103/PhysRevB.75.144508, confirmed by 13 papers
Doping variants (7)
| Formula | Tc max (K) | Tc amb. (K) | Papers | Doping |
|---|---|---|---|---|
| Bi2Sr2CaCu2Ox | 93.0 | 85.0 | 24 | 0.150 |
| Bi2Sr2CaCu2Oy | 92.2 | 91.0 | 30 | — |
| (Bi1-yPby)2Sr2CaCu2O8+x | 85.0 | — | 1 |
Evidence (1650 records from 1059 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 123.0 | — | — | — | — | 2009 | T1 | 0904.1223 |
| 120.0 | — | polycrystal | resistivity | — | 2017 | T1 | 1701.09124 |
| 120.0 | — |
Structure
- Crystal structure
- pseudotetragonal
- Space group
- D2h
- Lattice a (Å)
- 3.825
- Lattice c (Å)
- 30.810
Superconducting parameters
- Pairing symmetry
- d-wave
- Gap structure
- nodal
- Hc2
- 300.0 T (exceeds ~150 T, estimated by extrapolating low-T M_d-H curves)
- λ_eph (e–ph coupling)
- 4.00
- ρ_s (superfluid stiffness)
- 14.2 meV
Competing orders
- ρ(T) exponent
- 1.00
Samples & pressure
- Sample form
- single_crystal
- Substrate
- SrTiO3
- Pressure type
- none
- Doping type
- hole
- Doping level
- 0.160