← Back to search

α-FeAs-free SmFeAsO1-xFx by low temperature sintering with slow cooling

Masaya Fujioka, Saleem James Denholme, Toshinori Ozaki, Hiroyuki Okazaki, Keita Deguchi, Satoshi Demura, Hiroshi Hara, Tohru Watanabe, Hiroyuki Takeya, Takahide Yamaguchi, Hiroaki Kumakura, Yoshihiko Takano

arXiv:1303.1309 · DOI 10.7566/JPSJ.82.094707 · 2013-03-06 · Journal of the Physical Society of Japan

T1theoretical8 citations

Active bibliographic source — not scientific approval

Bibliographic access preserves source history; it does not approve extracted materials or validate reported claims. Review warnings on each occurrence separately.

Abstract

We obtained amorphous-FeAs-free SmFeAsO1-xFx using a low temperature sintering with slow cooling. SmFeAsO1-xFx is sintered at 980 °C for 40 hours and cooled slowly down to 600 °C. The low temperature sintering suppresses the formation of amorphous FeAs, and the slow cooling introduces much fluorine into SmFeAsO1-xFx. The superconductivity of this sample appears at 57.8 K and the superconducting volume fraction reaches 96 %. To study the change of fluorine concentration during the cooling process, samples are quenched by water at 950 °C, 900 °C, 850 °C, 800 °C, 750 °C and 700 °C. It is found that fluorine is substituted not only at the maximum heating temperature but also during the cooling process. The low temperature sintering with slow cooling is very effective to obtain a homogeneous SmFeAsO1-xFx with high fluorine concentration.

Source-reported materials — not catalogue approval

FormulaReported Tc (K)Pressure (GPa)Type
SmFeAsO1-xFx

Archive — visibility unverified

Source-occurrence policy only; no material identity or catalogue acceptance is inferred from the formula.

57.8Pressure not reportedonset